Title: Ativação alcalina em peças de cerâmica vermelha.
Other Titles: Alkaline activation in red ceramic tiles.
???metadata.dc.creator???: RAMOS, Sileide de Oliveira.
???metadata.dc.contributor.advisor1???: MENEZES, Romualdo Rodrigues de.
???metadata.dc.contributor.advisor-co1???: MACEDO, Reginaldo Severo de.
???metadata.dc.contributor.referee1???: NEVES, Gelmires de Araújo.
???metadata.dc.contributor.referee2???: SOUSA, Bianca Viana de.
Keywords: Bloco Cerâmico;Geopolimerização;Resistência Mecânica;Mechanical Resistance;Geopolymerization;Ceramic Block
Issue Date: 15-Sep-2010
Publisher: Universidade Federal de Campina Grande
Citation: RAMOS, S. de O. Ativação alcalina em peças de cerâmica vermelha. 2010. 49 f. Dissertação (Mestrado em Ciência e Engenharia de Materiais), Programa de Pós-Graduação em Ciência e Engenharia de Materiais, Centro de Ciências e Tecnologia, Universidade Federal de Campina Grande - Paraíba - Brasil, 2010. Disponível em: http://dspace.sti.ufcg.edu.br:8080/jspui/handle/riufcg/4153
???metadata.dc.description.resumo???: Geopolímeros ou materiais ativados alcalinamente constituem uma classe de materiais que possuem características e propriedades que vêm fazendo com que sejam utilizados em várias aplicações. A metacaulinita é um dos materiais mais utilizados para a síntese de geopolímeros, sendo encontrada em abundância em peças de cerâmica vermelha. Assim, o objetivo desta pesquisa foi ativar alcalinamente peças de cerâmica vermelha de modo a desenvolver material geopolimérico no seu interior e reforçar suas propriedades mecânicas. A argila foi beneficiada e caracterizada por difração de raios X de e determinação de sua composição química. Os corpos-de-prova foram obtidos por extrusão e queimados a 700 oC. Foi realizada a caracterização físicomecânica e mineralógica dos corpos queimados. Em seguida os corpos de prova foram submetidos à ativação alcalina por imersão em solução de NaOH. Foi avaliada a influência da concentração da solução, do tempo de imersão e da condição de cura na resistência mecânica dos corpos ativados alcalinamente. Avaliou-se a evolução do comportamento mecânico dos corpos ativados alcalinamente, determinando-se sua resistência mecânica após 30 e 60 dias. Com base nos resultados pode-se observar que o tempo de imersão não influencia o módulo de ruptura dos corpos curados em temperatura ambiente, enquanto a variação da concentração da solução de ativação alcalina aumenta o módulo de ruptura dos corpos curados em temperatura ambiente. Por outro lado, a concentração da solução de ativação alcalina não influencia o módulo de ruptura dos corpos curados a 60oC. A evolução do módulo de ruptura dos corpos ativados alcalinamente, com o decorrer do tempo de cura, depende da temperatura de cura e das condições de tratamento alcalino, sendo observado que os maiores módulos de ruptura são obtidos nos corpos submetidos a condições alcalinas mais severas e curados em temperatura ambiente.
Abstract: Geopolymers or alkaline activator materials are a class of materials that have characteristics and properties that are causing them to be used in various applications. The metakaolin is one of the most widely used materials for the synthesis of geopolymers being found in abundance in red ceramic pieces. Thus, the objective of this research was to activate alkaline red ceramic pieces in order to develop geopolymer material inside and enhance their mechanical properties. The clay was processed and characterized by X-ray diffraction and determination of its chemical composition. The bodies of the test piece was obtained by extrusion and fired at 700 oC. Was performed the physicalmechanical and mineralogical composition of burned bodies. Then the specimens used in evidence were submitted to activation by immersion in alkaline solution NaOH. We evaluated the influence of solution concentration, immersion time and the condition of curing on the mechanical strength of the bodies alkaline activator. We evaluated the evolution of mechanical behavior of bodies alkaline activator, to determine their mechanical strength after 30 and 60 days. Based on the results can be seen that the immersion time does not influence the modulus of rupture of the body cured at room temperature, while varying the concentration of alkaline activation solution increases the bending strength of the bodies cured at room temperature. Moreover, the concentration of alkaline activation solution does not influence the mechanical strength of cured bodies to 60 oC. The evolution of the modulus of rupture of the bodies alkaline activator, in the course of curing time depends on the curing temperature and conditions of alkaline treatment and observed that the highest modulus of rupture are obtained in bodies subjected to alkaline conditions and more severe cured at room temperature.
Keywords: Bloco Cerâmico
Geopolimerização
Resistência Mecânica
Mechanical Resistance
Geopolymerization
Ceramic Block
???metadata.dc.subject.cnpq???: Engenharia de Materiais e Metalúrgica
URI: http://dspace.sti.ufcg.edu.br:8080/jspui/handle/riufcg/4153
Appears in Collections:Mestrado em Ciência e Engenharia de Materiais.

Files in This Item:
File Description SizeFormat 
SILEIDE DE OLIVEIRA RAMOS - DISSERTAÇÃO PPG-CEMat CCT 2010.pdfSileide de Oliveira Ramos - Dissertação PPG-CEMat 20101.7 MBAdobe PDFView/Open


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.