Please use this identifier to cite or link to this item: http://dspace.sti.ufcg.edu.br:8080/jspui/handle/riufcg/6887
Title: Fotodegradação de termoplásticos semicristalinos.
Other Titles: Photodegradation of semicrystalline thermoplastics.
???metadata.dc.creator???: FECHINE, Guilhermino José Macêdo.
???metadata.dc.contributor.advisor1???: RABELLO, Marcelo Silveira.
???metadata.dc.contributor.referee1???: CARVALHO, Laura Hecker de.
???metadata.dc.contributor.referee2???: GARCIA , Rosângela Balaban.
Keywords: Plásticos;Termoplásticos;Fotodegradação;Envelhecimento Natural;Polímeros;Processos Degradativos;Termoplásticos Semicristalinos;Plastics;Thermoplastics;Photodegradation;Natural Aging;Polymers;Degradative Processes;Semicrystalline Thermoplastics
Issue Date: 15-Sep-1998
Publisher: Universidade Federal de Campina Grande
Citation: FECHINE, Guilhermino José Macedo. Fotodegradação de termoplásticos semicristalinos. 1998. 108 f. (Dissertação de Mestrado em Engenharia Química), Curso de Mestrado em Engenharia Química, Centro de Ciências e Tecnologia, Universidade Federal da Paraíba - Campus II Campina Grande - Brasil, 1998. Disponível em: http://dspace.sti.ufcg.edu.br:8080/jspui/handle/riufcg/6887
???metadata.dc.description.resumo???: Quando submetidos as intempéries naturais, os polímeros sofrem grandes alterações estruturais que resultam em deterioração no comportamento mecânico e em modificações na aparência superficial, frequentemente com a formação de fissuras e amarelamento. De acordo com a estrutura química do polímero e sua morfologia, a sensibilidade ao envelhecimento natural e bastante variada, ocorrendo modificações em suas propriedades desde poucos meses ate a alguns anos. A absorção da radiação ultra-violeta esta diretamente ligada com a estrutura química do polímero e das impurezas presentes, e esta energia absorvida pode resultar em cisão molecular, iniciando a degradação foto-oxidativa, reduzindo a vida útil do material. Este trabalho descreve os efeitos ambientais na degradabilidade de três poliolefinas: polipropileno (PP), polietileno de alta densidade (PEAD) e polietileno de baixa densidade (PEBD), e de um poliéster, o poli(tereftalato de etileno) (PET), sendo que este em estados cristalinos distintos, um amorfo (PET), e outro semi-cristalino (PETCRIS). Os corpos de prova foram expostos as intempéries em Campina Grande (PB) por um período de 38 semanas. Durante todo o período de exposição foram coletados diariamente dados de temperatura, precipitação, pluviometria, radiação solar e umidade. A caracterização das amostras foi feita através de modificações em propriedades mecânicas e térmicas, extensão da degradação química, índice de fluidez e analise de superfície de fratura.
Abstract: ABSTRACT When polymer products are exposed to the natural weathering, some structural changes occur in the molecules resulting in deterioration in mechanical properties and modification in surface appearance like yellowness and formation of surface cracks. The weatherability of polymer varies widely and depends on a number of factors like the polymer chemical structure and the presence of impurities, plays major role during photodegradation because it controls the initiation step wich ultimately results in chain scission. This work will describe the effects of natural photodegradation on the chemical structure and physical properties of threee types of polyolefins (polypropylene, high density polyethylene and low density polythylene) and two types of polyethylene terephthalate (amorphous and semi-crystalline). Samples were exposed the natural weathering in Campina Grande (PB) for periods of up to 38 weeks. At selected intervals they were analysed for mechanical and thermal properties, melt flow index, extent of chemical degradation and fracture suface. By comparing the results obtained for the three types of polyolefines it was observed that polypropylene was the most sensitive one showing changes in maximum elongation after only three weeks exposure whereas high density polyethylene did not show any sign of chemical degradation even after 38 weeks. On the other hand, low density polyethylene showed and intermediate behaviour and some evidence thet crosslinking reactions was formed during exposure. In the case of polyesters,
Keywords: Plásticos
Termoplásticos
Fotodegradação
Envelhecimento Natural
Polímeros
Processos Degradativos
Termoplásticos Semicristalinos
Plastics
Thermoplastics
Photodegradation
Natural Aging
Polymers
Degradative Processes
Semicrystalline Thermoplastics
???metadata.dc.subject.cnpq???: Engenharia Química.
URI: http://dspace.sti.ufcg.edu.br:8080/jspui/handle/riufcg/6887
Appears in Collections:Mestrado em Engenharia Química

Files in This Item:
File Description SizeFormat 
GUILHERMINO JOSÉ MACEDO FECHINE - DISSERTAÇÃO PPGEQ 1998.pdfGuilhermino José Macedo Fechine - Dissertação PPGEQ 1998. 6.83 MBAdobe PDFView/Open


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.