DSpace/Manakin Repository

Avaliação da susceptibilidade á fragilização por hidrogênio de juntas soldadas de aço API 5L XBO com diferentes combinações de consumíveis.

Mostrar registro simples

dc.creator.ID SOARES, E. P. pt_BR
dc.creator.Lattes http://lattes.cnpq.br/3557836810205502 pt_BR
dc.contributor.advisor1 MACIEL, Theophilo Moura.
dc.contributor.advisor1ID MACIEL, T. M. pt_BR
dc.contributor.advisor1Lattes http://lattes.cnpq.br/9476858938351846 pt_BR
dc.contributor.referee1 SANTOS, Marco Antônio dos.
dc.contributor.referee2 CASTRO, Walman Benício de.
dc.contributor.referee3 FERREIRA, Ricardo Arthur Sanguinetti.
dc.description.resumo Neste trabalho apresenta-se um estudo da susceptibilidade a fragilização peio hidrogênio de juntas soldadas de ago API 5L XBO, avaliando-sa a influência dos procedimentos, processo e consumíveis de soldagem. Foram utilizados os processes ao Arco El&trico com Eletrodo Revestido (SMAW), com Eletrodo de Tungstênio e Proteção de Gás Inerte (GTAW ou TIG) e com Arame Tubular (FCAW). Com relação aos consumíveis foram utilizados os eletrodos AWS E6010 para o passe de raiz e os eletrodos AWS E8Q10, E 9010, E8018 e E9018-G para os passes quentes e de enchimento no processo SMAW com eletrodos retirados da estufa e diretamente da caixa. O processo GTAW foi utilizado apenas para a soldagem do passe de raiz utilizand como consumíveis o arame AWS ER70S-3. No processo FCAW foram utilizados os consumíveis AWS E91T8-K8 auto protegido e WSE91T1-G este ultimo com proteção gasosa constituída de (Ar25). Os testes de fragilização per hidrogênio foram realizados de acordo com a norma ASTM G129-2006 com uma solução aquosa (solução A - NACE TM0177/2005), porem utilizando microadições de tiossulfato de sódio (Na2S203) em substituição ao borbulhamento de H2& De acordo com valores de afongamento, reduções de área e tempo de ruptura, foi possível observar que todas as juntas foram susceptíveis ao fundamento de fragilização por hidrogênio. Al6m do mais, todas as juntas apresentaram mudança nítida no modo de fratura em tração e apresentaram trincamento secundano sobre a superfície do corpo de prova. Estes resultados ainda foram associados a caracterização microestrutural do metal de solda e ao levantamento do perfil de dureza de cada junta; o que possibilitou avaliar o grau de influencia da mudança de consumíveis sobre o fundamento de fragilização por hidrogênio. Ao final dos resultados pode-se constatar que todas as fraturas ocorreram nos metais de solda, e que a junta que obteve o melhor resultado nos testes de fragilização; foi aquela soldada utilizando o processo GTAW no passe de raiz com o consumíveis AWS ER70S-3, o processo SMAW no passe quente com o consumíveis AWS E8010 e o processo FCAW nos passes de enchimento e acabamento, utilizando como consumiveis o arame AWSE91T1-G com proteção gasosa. Esta condição de soldagem apresentou para a região central do metal de solda o maior percentual de ferrita acicular (AF}~ (43%), o menor valor de dureza (147,6HV) e o melhor resultado para a Ração de Redução de Área (RRA)-(0,59), o que a identifica como sendo a junta soldada menos susceptível ao fenômeno de fragilização por hidrogênio. pt_BR
dc.publisher.country Brasil pt_BR
dc.publisher.department Centro de Ciências e Tecnologia - CCT pt_BR
dc.publisher.program PÓS-GRADUAÇÃO EM CIÊNCIA E ENGENHARIA DE MATERIAIS pt_BR
dc.publisher.initials UFCG pt_BR
dc.subject.cnpq Engenharia de Materiais
dc.title Avaliação da susceptibilidade á fragilização por hidrogênio de juntas soldadas de aço API 5L XBO com diferentes combinações de consumíveis. pt_BR
dc.date.issued 2011-12-09
dc.description.abstract This paper presents a study of susceptibility to embrittlement by API 5L XBO welded gaskets, evaluating the influence of welding procedures, process and consumables. Were used the Processes with Coated Electrode (SMAW), with Tungsten and Inert Gas Protection (GTAW or TIG) and Tubular Wire (FCAW). For consumables, AWS E6010 electrodes were used. for the root pass and the AWS E8Q10, E 9010, E8018 and E9018-G electrodes for hot and filling passes in the SMAW process with electrodes removed from the greenhouse and directly from the box. The GTAW process was used only for the root pass welding using AWS ER70S-3 wire as consumables. In the FCAW process AWS E91T8-K8 consumables were used. self-shielding and AWSE91T1-G the latter with gas shielding consisting of (Ar25). The hydrogen perilization tests were performed according to the ASTM G129-2006 standard with an aqueous solution (solution A - NACE TM0177 / 2005), but using sodium thiosulfate microadditions (Na2S203) instead of bubbling H2 & According to values ​​of reduction, area reductions and rupture time, it was observed that all the joints were susceptible to hydrogen embrittlement grounds. Al6m from In addition, all joints showed a distinct change in tensile fracture mode. and presented secondary cracking on the specimen surface. These results were still associated with the microstructural characterization of weld metal and lifting the hardness profile of each joint; what made it possible to evaluate the degree of influence of the change of consumables on the hydrogen embrittlement foundation. At the end of the results it can be verified that all fractures occurred in the weld metals, and that the joint that obtained the better result in embrittlement tests; was that welded using the GTAW process from scratch with AWS ER70S-3 consumables, the process SMAW in the hot pass with AWS E8010 consumables and the FCAW process in the filling and finishing passes using wire as consumables AWSE91T1-G with gas protection. This welding condition presented for the central region of the weld metal the highest percentage of acicular ferrite (AF} ~ (43%), the lowest hardness value (147.6HV) and the best result for the Ration of Area Reduction (RRA) - (0.59), which identifies it as the welded joint less susceptible to the phenomenon of hydrogen embrittlement. pt_BR
dc.identifier.uri http://dspace.sti.ufcg.edu.br:8080/jspui/handle/riufcg/10593
dc.date.accessioned 2020-01-02T15:09:23Z
dc.date.available 2020-01-02
dc.date.available 2020-01-02T15:09:23Z
dc.type Dissertação pt_BR
dc.subject Aço API 5L X80
dc.subject Juntas Soldadas
dc.subject Fragilização por Hidrogênio
dc.subject Microestrutura
dc.subject Microdureza
dc.subject Metal de Base
dc.subject Metal de Solda
dc.subject API 5L X80 Steel
dc.subject Welded Joints
dc.subject Hydrogen Embrittlement
dc.subject Microstructure
dc.subject Microhardness
dc.subject Welding Metal
dc.subject Base Metal
dc.rights Acesso Aberto pt_BR
dc.creator SOARES, Emanuel Pereira.
dc.publisher Universidade Federal de Campina Grande pt_BR
dc.language por pt_BR
dc.relation.references SOARES, Emanuel Pereira. Avaliação da susceptibilidade á fragilização por hidrogênio de juntas soldadas de aço API 5L XBO com diferentes combinações de consumíveis.2011. 119F (Dissertação) Mestrado em Ciência e Engenharia de Materiais, Programa de Pós-graduação em Ciência e Engenharia de Materiais, Centro de Ciências e Tecnologia, Universidade Federal de Campina Grande - Campina Grande - Paraíba - Brasil, 2011. Disponível em: http://dspace.sti.ufcg.edu.br:8080/jspui/handle/riufcg/10593 pt_BR
dc.title.alternative Evaluation of the susceptibility to hydrogen embrittlement of welded joints of api5l-x80 steel with different consumable combinations. pt_BR