dc.creator.ID |
NOBREGA, R. B. |
pt_BR |
dc.creator.ID |
DA NOBREGA, RAPHAEL B. |
pt_BR |
dc.creator.ID |
DA NÓBREGA, RAPHAEL BORGES. |
pt_BR |
dc.creator.Lattes |
http://lattes.cnpq.br/8566102268241861 |
pt_BR |
dc.contributor.advisor1 |
COSTA, Edson Guedes. |
|
dc.contributor.advisor1ID |
COSTA, E. G. |
pt_BR |
dc.contributor.advisor1ID |
Costa, E. G. |
pt_BR |
dc.contributor.advisor1ID |
E. C. Guedes. |
pt_BR |
dc.contributor.advisor1Lattes |
http://lattes.cnpq.br/3930289115658143 |
pt_BR |
dc.contributor.advisor2 |
GERMANO, André Dantas. |
|
dc.contributor.advisor2ID |
GERMANO, A. D. |
pt_BR |
dc.contributor.advisor2ID |
GERMANO, André Dantas. |
pt_BR |
dc.contributor.advisor2ID |
Germano, André D. |
pt_BR |
dc.contributor.advisor2Lattes |
http://lattes.cnpq.br/5861671113603396 |
pt_BR |
dc.contributor.referee1 |
LOPES, Ivan José da silva. |
|
dc.contributor.referee1ID |
LOPES, I. J. S. |
pt_BR |
dc.contributor.referee1ID |
Lopes, I. |
pt_BR |
dc.contributor.referee1ID |
da Silva Lopes, Ivan Jose. |
pt_BR |
dc.contributor.referee1Lattes |
http://lattes.cnpq.br/2586046683895112 |
pt_BR |
dc.contributor.referee2 |
ALTAFIM, Ruy Alberto Correa. |
|
dc.contributor.referee2ID |
ALTAFIM, R. A. C. |
pt_BR |
dc.contributor.referee2ID |
Altafim, Ruy Alberto Corrêa. |
pt_BR |
dc.contributor.referee2ID |
Corrêa Altafim, Ruy Alberto. |
pt_BR |
dc.contributor.referee2Lattes |
http://lattes.cnpq.br/3276653731957888 |
pt_BR |
dc.contributor.referee3 |
COSTA, Ana Cristina Figueiredo de Melo. |
|
dc.contributor.referee3ID |
COSTA, A. C. F. M. |
pt_BR |
dc.contributor.referee3ID |
DE MELO COSTA, ANA CRISTINA FIGUEIREDO. |
pt_BR |
dc.contributor.referee3ID |
Ana Cristina F. de M. Costa. |
pt_BR |
dc.contributor.referee3Lattes |
http://lattes.cnpq.br/6309225172752964 |
pt_BR |
dc.contributor.referee4 |
FERREIRA, Tarso Vilela. |
|
dc.contributor.referee4ID |
FERREIRA, T. V. |
pt_BR |
dc.contributor.referee4ID |
FERREIRA, TARSO V. |
pt_BR |
dc.contributor.referee4ID |
FERREIRA, TARSO. |
pt_BR |
dc.contributor.referee4Lattes |
http://lattes.cnpq.br/9395719025602516 |
pt_BR |
dc.contributor.referee5 |
NEVES, Washington Luiz Araújo. |
|
dc.contributor.referee5ID |
NEVES, W. L. A. |
pt_BR |
dc.contributor.referee5ID |
NEVES, WASHINGTON L.A. |
pt_BR |
dc.contributor.referee5ID |
NEVES, W. L. A. |
pt_BR |
dc.contributor.referee5Lattes |
http://lattes.cnpq.br/3107104665517286 |
pt_BR |
dc.description.resumo |
Neste trabalho foi investigada a influência da cera de carnaúba na composição de
revestimentos de silicone aplicados no isolamento externo em sistemas de alta tensão.
Os compósitos foram constituídos por borracha de silicone vulcanizável a temperatura
ambiente acrescida de diferentes concentrações de alumina tri-hidratada e da cera de
carnaúba. A morfologia e distribuição das cargas nos compósitos foram analisadas por
meio de imagens de microscopia eletrônica de varredura. A estrutura química da cera de
carnaúba e de revestimentos de RTV-SIR foi caracterizada por meio dos espectros de
absorção na região do infravermelho. Os efeitos da polarização e resistência à ruptura
elétrica foram analisados a partir de medições da constante dielétrica e rigidez
dielétrica. Ensaios de envelhecimento acelerado foram realizados por meio da exposição
à radiação UV e aplicação de estresses elétricos em função do tempo. A suportabilidade
dielétrica de isoladores revestidos com as composições investigadas foi avaliada a partir
da aplicação de sucessivas descargas disruptivas para diferentes níveis de poluição.
O estado do isolamento após o ensaio foi determinado a partir de medições da corrente
da fuga. A resistência aos fenômenos de trilhamento elétrico e erosão foi avaliada para
amostras dos compósitos estudados. Os efeitos provocados pela exposição de amostras
dos compósitos à radiação UV foram avaliados por meio de variações na
hidrofobicidade e nos espectros de FTIR. A partir dos resultados, foi verificado que a
exposição à radiação ultravioleta ocasiona uma redução nos valores de ângulo de
contato para amostras do material investigado. Amostras adicionadas da cera de
carnaúba em concentrações mássicas até 10% apresentaram boa suportabilidade
dielétrica em condições de poluição, baixos valores de correntes de fuga para ensaios de
névoa após a aplicação de descargas disruptivas e resistência à ocorrência do
trilhamento elétrico e erosão. Os melhores desempenhos foram obtidos para as
composições adicionadas de cera de carnaúba e alumina tri-hidratada em concentrações
de 5% e 20%, respectivamente. |
pt_BR |
dc.publisher.country |
Brasil |
pt_BR |
dc.publisher.department |
Centro de Engenharia Elétrica e Informática - CEEI |
pt_BR |
dc.publisher.program |
PÓS-GRADUAÇÃO EM ENGENHARIA ELÉTRICA |
pt_BR |
dc.publisher.initials |
UFCG |
pt_BR |
dc.subject.cnpq |
Engenharia Elétrica |
pt_BR |
dc.title |
Influência da cera de carnasúba do desempenho de revestimento de silicone aplicados no isolamento externo. |
pt_BR |
dc.date.issued |
2019-09-24 |
|
dc.description.abstract |
In this work the influence of carnauba wax on the composition of silicone coatings
applied to outdoor insulation in high voltage systems was investigated. The composites
were contained of vulcanizable silicone rubber at room temperature added with different
concentrations of alumina trihydrate and carnauba wax. The morphology and filler
distribution in the composites were analyzed by SEM. The chemical structure of
carnauba wax and RTV-SIR coatings was characterized by the infrared spectrum of
absorption. The effects of polarization and resistance to electrical rupture were analyzed
from measurements of dielectric constant and dielectric strength. Accelerated aging
tests were performed through the exposure to UV radiation and application of electrical
stresses as a function of time. The dielectric supportability of insulators coated with the
investigated compositions was evaluated through the application of successive
disruptive discharges with different levels of pollution. The state of isolation after the
test was determined from leakage current measurements. The resistance to the electrical
tracking and erosion phenomena was evaluated for composite samples. The length of
the tracking, the eroded mass and leakage current measurements were used as
parameters of the analysis. The effects caused by exposure of composite samples to UV
radiation were evaluated by variations in hydrophobicity and FTIR spectrum. From the
results, it was verified that the exposure to ultraviolet radiation causes a reduction in the
contact angle values for samples of the investigated material. Samples containing
carnauba wax at mass concentrations up to 10% showed good dielectric supportability
in pollution conditions, low leakage current values in fog tests realized after the
application of disruptive discharges and resistance to electrical tracking and erosion.
The best performances were obtained for the compositions filled carnauba wax and
alumina trihydrate compositions at concentrations of 5% and 20%, respectively. |
pt_BR |
dc.identifier.uri |
http://dspace.sti.ufcg.edu.br:8080/jspui/handle/riufcg/27187 |
|
dc.date.accessioned |
2022-09-14T14:36:56Z |
|
dc.date.available |
2022-09-14 |
|
dc.date.available |
2022-09-14T14:36:56Z |
|
dc.type |
Tese |
pt_BR |
dc.subject |
Isolamento externo em sistema de alta tensão- revestimento de silicone |
pt_BR |
dc.subject |
Cera de Carnaúba |
pt_BR |
dc.subject |
Isoladores |
pt_BR |
dc.subject |
Borracha de silicone |
pt_BR |
dc.subject |
Radiação UV |
pt_BR |
dc.subject |
Trilhamento elétrico |
pt_BR |
dc.subject |
Suportabilidade dielétrica |
pt_BR |
dc.subject |
Constante dielétrica |
pt_BR |
dc.subject |
FTIR |
pt_BR |
dc.subject |
Caorrente de fung |
pt_BR |
dc.subject |
Aluminum trihydrate |
pt_BR |
dc.subject |
External insulation in high voltage system - silicone coating |
pt_BR |
dc.subject |
Carnauba wax |
pt_BR |
dc.subject |
Insulators |
pt_BR |
dc.subject |
Silicone rubber |
pt_BR |
dc.subject |
UV radiation |
pt_BR |
dc.subject |
Electric track |
pt_BR |
dc.subject |
Dielectric withstand |
pt_BR |
dc.subject |
Dielectric constant |
pt_BR |
dc.subject |
Fung flow |
pt_BR |
dc.subject |
Aluminum trihydrate |
pt_BR |
dc.rights |
Acesso Aberto |
pt_BR |
dc.creator |
NOBREGA, Raphael Borges da. |
|
dc.publisher |
Universidade Federal de Campina Grande |
pt_BR |
dc.language |
por |
pt_BR |
dc.title.alternative |
Influência da cera de carnasúba do desempenho de revestimento de silicone aplicados no isolamento externo. |
pt_BR |
dc.identifier.citation |
NOBREGA, Raphael Borges da. Influência da cera de carnaúba do desempenho de revestimento de silicone aplicados no isolamento externo. 2019. 133 fl. Tese (Doutorado em Engenharia Elétrica), Programa de Pós-Graduação em Engenharia Elétrica, Centro de Engenharia Elétrica e Informática, Universidade Federal de Campina Grande - Paraíba - Brasil, 2019. |
pt_BR |