Repositorio Dspace/Manakin

Deposição de revestimento AISI 317L contra corrosão por processo GTAW mecanizado com adição de arame frio.

Mostrar el registro sencillo del ítem

dc.creator.ID SANTOS, R. B. C. pt_BR
dc.creator.Lattes http://lattes.cnpq.br/3960722864174263 pt_BR
dc.contributor.advisor1 SANTANA, Renato Alexandre Costa de.
dc.contributor.advisor1ID SANTANA, R. A. C. pt_BR
dc.contributor.advisor1Lattes http://lattes.cnpq.br/1438381290031148 pt_BR
dc.contributor.advisor-co1 SILVA, Marcos Mesquita da.
dc.contributor.advisor-co1ID SILVA, MARCOS MESQUITA DA. pt_BR
dc.contributor.advisor-co1Lattes http://lattes.cnpq.br/4819493317308583 pt_BR
dc.contributor.referee1 MACIEL, Theophilo Moura.
dc.contributor.referee1ID MACIEL, T. M. pt_BR
dc.contributor.referee1Lattes http://lattes.cnpq.br/9476858938351846 pt_BR
dc.contributor.referee2 MELO, Raphael Henrique Falcão de.
dc.contributor.referee2ID MELO, R. H. F. pt_BR
dc.contributor.referee2Lattes http://lattes.cnpq.br/9758661753469822 pt_BR
dc.description.resumo O presente trabalho tem como objetivo investigar a resistência à corrosão de revestimentos de aço inoxidável austenítico aplicados em substrato de aço carbono via processo GTAW mecanizado com adição de arame frio (GTAW-MAF). As soldagens foram realizadas utilizando como o metal de adição arames do aço AISI 317L, com diâmetro de 1,2mm. Inicialmente, foi realizado um estudo sistemático de cordões de solda isolados a fim de investigar o efeito dos parâmetros de soldagem na geometria e diluição desses cordões. Para isso, foi traçado um planejamento de experimentos fatorial linear com três variáveis independentes (corrente, velocidade de alimentação e distância eletrodo/peça) além da adição de pontos centrais e axiais (23+6+3), totalizando 17 ensaios. As variáveis respostas analisadas foram diluição (%), molhabilidade (°), altura e largura dos cordões (mm), selecionando três experimentos com a melhor viabilidade operacional para serem utilizados no processo de revestimento. No processo de soldagem de revestimentos utilizou-se duas técnicas: com e sem preaquecimento do substrato. A temperatura de preaquecimento utilizada foi de 150oC. Para os cordões isolados, obteve- se alturas entre 1,87 e 5,03mm, larguras entre 6,79 e 13,03mm, molhabilidades entre 51,60 e 133,65o e diluições entre 5,65 e 47,82%. O preaquecimento mostrou-se eficaz na diminuição de descontinuidades entre cordões e conseguiu-se desenvolver uma técnica satisfatória e replicável para a deposição de revestimento AISI 317L via processo GTAW- MAF. Verificou-se que o processo de deposição utilizado conferiu revestimentos com composição química semelhantes às do material de adição utilizado e que os melhores resultados de resistência à corrosão e diluição se deram ao utilizar correntes de soldagem acima de 220A, velocidade de alimentação entre 4m/min e 5m/min e distância do eletrodo para a peça de 10mm. O revestimento R2T2 apresentou bons resultados de diluição (10,38%), resistência à polarização 2,8x maior em relação ao substrato, pouca presença de inclusões e boa regularidade operacional na deposição dos cordões com baixa presença de descontinuidades. pt_BR
dc.publisher.country Brasil pt_BR
dc.publisher.department Centro de Ciências e Tecnologia - CCT pt_BR
dc.publisher.program PÓS-GRADUAÇÃO EM ENGENHARIA MECÂNICA pt_BR
dc.publisher.initials UFCG pt_BR
dc.subject.cnpq Engenharia Mecânica pt_BR
dc.title Deposição de revestimento AISI 317L contra corrosão por processo GTAW mecanizado com adição de arame frio. pt_BR
dc.date.issued 2021-12-23
dc.description.abstract The present work aims to investigate the corrosion resistance of austenitic stainless steel coatings applied on carbon steel substrate via mechanized GTAW process with the addition of cold wire (GTAW-MAF). The welds were carried out using AISI 317L steel wires with a diameter of 1.2mm as the filler metal. For the isolated welding beads, a linear factorial design experiment was designed with three independent variables (current, feed speed and electrode/part distance) and with the addition of central and axial points (23+6+3), totaling 17 tests . The response variables analyzed were dilution (%), wettability (°), height and width of beads (mm), selecting the three parameters with the best operational feasibility to be used in the coating process. In the welding coatings process, two techniques were used: with and without substrate preheating. Preheating proved to be effective in reducing discontinuities between weld beads and it was possible to develop a viable and replicable technique for the deposition of AISI 317L coating via the GTAW-MAF process. It was found that the deposition process used provided coatings with chemical composition similar to those of the addition material used and that the best results in corrosion resistance and dilution were given when using welding currents above 220A, feed speed between 4m/min and 5m/min and electrode-to-part distance of 10mm. The R2T2 coating showed good dilution results (10.38%), resistance to polarization 2.8x greater in relation to the substrate, little presence of inclusions and good operational regularity in the deposition of beads with low presence of discontinuities. pt_BR
dc.identifier.uri http://dspace.sti.ufcg.edu.br:8080/jspui/handle/riufcg/29231
dc.date.accessioned 2023-04-04T14:39:55Z
dc.date.available 2023-04-04
dc.date.available 2023-04-04T14:39:55Z
dc.type Dissertação pt_BR
dc.subject Soldagem de revestimento pt_BR
dc.subject AISI 317L pt_BR
dc.subject Corrosão pt_BR
dc.subject GTAW- MAF pt_BR
dc.subject Aço Inoxidável austenítico pt_BR
dc.subject Overlay welding pt_BR
dc.subject Corrosion pt_BR
dc.subject Austenitic stainless steel pt_BR
dc.subject Soldadura de superposición pt_BR
dc.subject Acero inoxidable austenitico pt_BR
dc.rights Acesso Aberto pt_BR
dc.creator SANTOS, Rafael Barbosa Carneiro dos.
dc.publisher Universidade Federal de Campina Grande pt_BR
dc.language por pt_BR
dc.title.alternative AISI 317L coating deposition against process corrosion Mechanized GTAW with addition of cold wire. pt_BR
dc.title.alternative Deposición de recubrimiento AISI 317L contra la corrosión del proceso GTAW mecanizado con adición de hilo frío. pt_BR
dc.identifier.citation SANTOS, Rafael Barbosa Carneiro dos. Deposição de revestimento AISI 317L contra corrosão por processo GTAW mecanizado com adição de arame frio. 2022. 114fl. (Dissertação de Mestrado), Programa de Pós-Graduação em Engenharia Mecânica, Centro de Ciências e Tecnologia, Universidade Federal de Campina Grande - Paraíba - Brasil, 2019. Disponível em:http://dspace.sti.ufcg.edu.br:8080/jspui/handle/riufcg/29231 pt_BR
dc.description.resumen El presente trabajo tiene como objetivo investigar la resistencia a la corrosión de Recubrimientos de acero inoxidable austenítico aplicados al sustrato de acero al carbono a través de Proceso GTAW mecanizado con adición de hilo frío (GTAW-MAF). las soldaduras se realizaron utilizando alambres de acero AISI 317L como metal de aporte, con 1,2 mm de diámetro. Inicialmente, se llevó a cabo un estudio sistemático de los cordones de soldadura. aislado para investigar el efecto de los parámetros de soldadura en la geometría y la dilución de estos cordones. Para ello se diseñó un diseño factorial lineal de experimentos con tres variables independientes (corriente, velocidad de avance y distancia electrodo/pieza) además de la suma de puntos centrales y axiales (23+6+3), totalizando 17 ensayo. Las variables de respuesta analizadas fueron dilución (%), humectabilidad (°), altura y ancho del cordón (mm), seleccionando tres experimentos con la mejor viabilidad operativo para ser utilizado en el proceso de recubrimiento. En el proceso de soldadura de recubrimientos se utilizaron dos técnicas: con y sin precalentamiento del sustrato. A La temperatura de precalentamiento utilizada fue de 150oC. Para los hilos aislados se obtuvo si alturas entre 1,87 y 5,03 mm, anchos entre 6,79 y 13,03 mm, humectabilidad entre 51,60 y 133,65o y diluciones entre 5,65 y 47,82%. El precalentamiento demostró ser efectivo en reducción de discontinuidades entre cuerdas y fue posible desarrollar una técnica satisfactorio y replicable para la deposición de recubrimiento AISI 317L a través del proceso GTAW MAF. Se encontró que el proceso de deposición utilizado proporcionó recubrimientos con composición química similar a la del material de relleno utilizado y que la mejor Se obtuvieron resultados de resistencia a la corrosión y dilución al usar corrientes de soldadura por encima de 220A, velocidad de avance entre 4m/min y 5m/min y distancia de electrodos para la pieza de 10 mm. El recubrimiento R2T2 mostró buenos resultados de dilución. (10,38%), resistencia a la polarización 2,8x mayor respecto al sustrato, poca presencia de inclusiones y buena regularidad operativa en la deposición de cordones con baja presencia de discontinuidades. pt_BR


Ficheros en el ítem

Este ítem aparece en la(s) siguiente(s) colección(ones)

Mostrar el registro sencillo del ítem

Buscar en DSpace


Búsqueda avanzada

Listar

Mi cuenta