DSpace/Manakin Repository

Influência da umidade e da microestrutura na formação de trincas induzidas pelo hidrogênio no metal de solda.

Mostrar registro simples

dc.creator.Lattes http://lattes.cnpq.br/5692770225933017 pt_BR
dc.contributor.advisor1 KIMINAMI, Claudio Shyinti
dc.contributor.advisor1ID KIMINAMI, C. S. pt_BR
dc.contributor.advisor1Lattes http://lattes.cnpq.br/5443002033733395 pt_BR
dc.contributor.advisor2 ALCÂNTARA, Nelson Guedes de.
dc.contributor.advisor2 SANTOS, Marco Antonio dos.
dc.contributor.advisor2ID SANTOS, M. A.
dc.contributor.advisor2ID ALCÂNTARA, N. G.
dc.contributor.advisor2Lattes http://lattes.cnpq.br/3123107570992184
dc.contributor.advisor2Lattes http://lattes.cnpq.br/4825985900425353
dc.contributor.referee1 LIMA, Severino Jackson Guedes de.
dc.description.resumo Neste trabalho avaliou-se o teor de unidade contido no revestimento dos eletrodos AWS E 8018 e AWS E 1018 na condição de ressecado e, quando expostos às condições ambientais e condições controladas de temperatura e umidade relativa. Os resultados demonstram a grande sensibilidade da taxa de absorção de umidade, com alteração na temperatura e/ou umidade relativa sendo que, os níveis máximos estabelecidos pelas normas são atingidos em poucas horas de exposição a condições normais do ambiente. Para avaliação da influência da umidade assim adquirida, no aparecimento de trincas a frio induzidas pelo hidrogênio no metal de solda, ensaios TEKKEN, com chanfro em Y simétrico, foram realizados com chapas de aço ASTMA 516 - gr 65.0 teor de umidade total variou de 0.19% até 3.04% e a energia de 0.74 kJ/mm a 2.27 kJ/mm. Não se verificou o aparecimento de trincas com o eletrodo AWS E 8018 que apresentou um grande percentual de ferrita acicular. Com o AWS E 1018, as trincas surgiram quando condições críticas de umidade total e aporte de calor foram utilizados. Um nível mínimo de energia em torno de 1.6kJ/mm foi necessário para se evitar trincas, mesmo como eletrodos ressecados. Nessas amostras o percentual de ferrita acicular não foi tão grande, entretanto uma quantidade significativa de ferrita primária formou-se. pt_BR
dc.publisher.country Brasil pt_BR
dc.publisher.department Centro de Engenharia Elétrica e Informática - CEEI pt_BR
dc.publisher.program PÓS-GRADUAÇÃO EM ENGENHARIA ELÉTRICA pt_BR
dc.publisher.initials UFCG pt_BR
dc.subject.cnpq Engenharia Elétrica
dc.title Influência da umidade e da microestrutura na formação de trincas induzidas pelo hidrogênio no metal de solda. pt_BR
dc.date.issued 1992-03-11
dc.description.abstract In this work the unit content contained in the coating of the AWS electrodes E 8018 and AWS E 1018 in the condition of dried and, when exposed to the ambient conditions and controlled conditions of temperature and relative humidity, was evaluated. The results demonstrate the high sensitivity of the moisture absorption rate, with changes in temperature and / or relative humidity, where the maximum levels established by the standards are reached in a few hours of exposure to normal environmental conditions. In order to evaluate the influence of the humidity thus obtained, in the appearance of cold cracks induced by the hydrogen in the weld metal, TEKKEN tests, with symmetrical Y bevel, were performed with steel plates ASTMA 516 - gr 65.0 total moisture content ranged from 0.19 % to 3.04% and the energy from 0.74 kJ / mm to 2.27 kJ / mm. No cracking was observed with the AWS E 8018 electrode, which presented a high percentage of acicular ferrite. With AWS E 1018, cracks arose when critical conditions of total moisture and heat input were used. A minimum energy level of around 1.6 kJ / mm was required to avoid cracking, even as dry electrodes. In these samples the percentage of acicular ferrite was not so great, however a significant amount of primary ferrite formed. pt_BR
dc.identifier.uri http://dspace.sti.ufcg.edu.br:8080/jspui/handle/riufcg/4143
dc.date.accessioned 2019-06-05T16:09:06Z
dc.date.available 2019-06-05
dc.date.available 2019-06-05T16:09:06Z
dc.type Dissertação pt_BR
dc.subject Umidade.
dc.subject Metal de Solda.
dc.subject Eletrodos AWS e 8018.
dc.subject Eletrodos AWS e 10018.
dc.subject Projetos de Produtos Mecânicos.
dc.subject Moisture.
dc.subject Welding Metal.
dc.subject AWS and 8018 Electrodes.
dc.subject AWS and 10018 Electrodes.
dc.subject Mechanical Products Projects.
dc.rights Acesso Aberto pt_BR
dc.creator SILVA, Egberto Pedro da.
dc.publisher Universidade Federal de Campina Grande pt_BR
dc.language por pt_BR
dc.title.alternative Influence of moisture and microstructure on the formation of hydrogen-induced cracks in the weld metal. pt_BR
dc.identifier.citation SILVA, Egberto Pedro da. Influência da umidade e da microestrutura na formação de trincas induzidas pelo hidrogênio no metal de solda. 1992. 91f. (Dissertação) Mestrado em Engenharia Mecânica, Curso de Pós-Graduação em Engenharia Mecânica, Centro de Ciências e Tecnologia, Universidade Federal da Paraíba – Campus II - Campina Grande - PB - Brasil, 1992. pt_BR