DSpace/Manakin Repository

Avaliação da resistência ao desgaste de revestimentos duros aplicados por soldagem em martelos trituradores de baterias automotivas.

Mostrar registro simples

dc.creator.ID SOUSA NETO, Emydio Clemente pt_BR
dc.creator.Lattes http://lattes.cnpq.br/6765388320260420 pt_BR
dc.contributor.advisor1 MACIEL, Theophilo Moura.
dc.contributor.advisor1ID MACIEL, T. M. pt_BR
dc.contributor.advisor1Lattes http://lattes.cnpq.br/9476858938351846 pt_BR
dc.contributor.advisor2 SANTOS, Marco Antonio dos.
dc.contributor.advisor2ID SANTOS, M. A. pt_BR
dc.contributor.advisor2Lattes http://lattes.cnpq.br/4825985900425353 pt_BR
dc.contributor.referee1 ARAÚJO, Carlos José de.
dc.contributor.referee2 MELO, João Baptista da Costa Agra.
dc.description.resumo O desgaste prematuro de conjuntos e componentes industriais, bem como de uma infinidade de outros segmentos, representa um grande fator para a redução da eficiência operacional de um equipamento, provocando assim, um aumento das perdas, e consequentemente, em altas despesas com manutenção e reposição de componentes mecânicos. Este trabalho aborda uma análise comparativa entre a resistência ao desgaste de martelos trituradores de baterias recuperados por três ligas a base de cobalto (Stellite 1, 6 e 21), bem como dois processos de deposição: os processos ao Arco Elétrico com Eletrodo Revestido (SMAW) e ao Arco Plasma Transferido com adição de Pó (PTA-P). Os martelos trituradores são originalmente confeccionados em aço inoxidável AISI 316 L sem nenhum recobrimento. Além da avaliação da resistência ao desgaste no próprio meio de trabalho foram realizados ensaios de microdureza, análises microestruturais via microscopia ótica, e eletrônica de varredura e, análise de diluição com o objetivo de caracterizar e consolidar a pesquisa para que se tenha o estudo comparativo da melhor liga e melhor processo de deposição. Os resultados demostraram que a melhor condição testada foi aquela que empregou a liga Stellite 6 depositadas pelo processo PTA-P. Essa condição apresentou a menor perda de massa nos ensaios de resistência ao desgaste, enquanto que a condição menos favorável foi verificada para os depósitos executados com a liga Stellite 1 utilizando o mesmo processo de deposição. A diluição média das ligas depositadas pelo processo SMAW foi 3,7 vezes maior do que a média apresentada utilizando o processo PTA-P. Os maiores valores de microdureza foram aqueles apresentados pelo revestimento executados com a liga Stellite 1 com maior teor de C, e esta liga, proporcionou um maior número de destacamento dos revestimentos. A microestrutura dos depósitos executados pelo processo PTA-P apresentou-se mais refinada quando comparada com aquelas depositadas pelo processo SMAW. pt_BR
dc.publisher.country Brasil pt_BR
dc.publisher.department Centro de Ciências e Tecnologia - CCT pt_BR
dc.publisher.program PÓS-GRADUAÇÃO EM ENGENHARIA MECÂNICA pt_BR
dc.publisher.initials UFCG pt_BR
dc.subject.cnpq Ciências pt_BR
dc.subject.cnpq Engenharia Mecânica pt_BR
dc.title Avaliação da resistência ao desgaste de revestimentos duros aplicados por soldagem em martelos trituradores de baterias automotivas. pt_BR
dc.date.issued 2015-07-31
dc.description.abstract The premature wear sets and industrial components, as well as many of other segments, is a big factor for reducing operational efficiency of equipment, thus causing an increase in losses, and consequently in high cost of maintenance and replacement of mechanical components. This work presents a comparative analysis of the wear resistance of AISI 316 L steel automotive batteries crushers hammers repaired by welding process using three cobalt-based alloys: Stellite 1, 6 and 21, as well as, two welding deposition process: Shielded Metal Arc Welding (SMAW) and Plasma Transferred Arc with addition powder (PTA-P). Crushers hammers are originally made of stainless steel AISI 316 L with no coating. Besides the “in situ” wear resistance evaluation microhardness tests, microstructure and dilution analysis by optical microscopy and scanning electron were done to characterize and consolidate research in order to have a comparative study of best league and better deposition process. The results showed that the best alloy was Stellite 6 using the PTA-P process, which had the lowest mass loss in wear resistance tests, while the less favorable condition was for deposits made with the alloy Stellite 1 using the same deposition welding process. The average dilution of the alloys deposited by the SMAW process was 3.7 times higher than the average using the PTA-P process. The highest microhardness values were presented by Stellite 1 alloy deposit, with higher C content, which also provided a greater number of coating detachment. The deposits made by the process PTAP showed a more refined microstructure when compared to those deposited by the SMAW process pt_BR
dc.identifier.uri http://dspace.sti.ufcg.edu.br:8080/jspui/handle/riufcg/452
dc.date.accessioned 2018-04-23T10:51:37Z
dc.date.available 2018-04-23
dc.date.available 2018-04-23T10:51:37Z
dc.type Dissertação pt_BR
dc.subject Resistência ao Desgaste pt_BR
dc.subject Revestimentos Duros pt_BR
dc.subject Ligas à Base de Cobalto pt_BR
dc.subject Processo PTA-P e SMAW pt_BR
dc.subject Martelos Trituradores de Baterias Automotivas pt_BR
dc.subject Wear Resistance pt_BR
dc.subject Hardfacing pt_BR
dc.subject Cobalt Alloys pt_BR
dc.subject PTA-P and SMAW Process pt_BR
dc.subject Hammers Crushers Automotive Batteries pt_BR
dc.rights Acesso Aberto pt_BR
dc.creator SOUSA NETO, Emydio Clemente de.
dc.publisher Universidade Federal de Campina Grande pt_BR
dc.language por pt_BR
dc.identifier.citation SOUSA NETO, E. C. de. Avaliação da resistência ao desgaste de revestimentos duros aplicados por soldagem em martelos trituradores de baterias automotivas. 2015. 102f. Dissertação (Mestrado em Engenharia Mecânica) – Programa de Pós-Graduação em Engenharia Mecânica, Centro de Ciências e Tecnologia, Universidade Federal de Campina Grande, Paraíba, Brasil, 2015. Disponível em: http://dspace.sti.ufcg.edu.br:8080/jspui/handle/riufcg/452 pt_BR